Process Data set: cement production;cement, portland cement, 42.5MPa;shaft kiln (en) en zh

Key Data Set Information
Location HLJ-CN
Reference year 2008
Name
cement production;cement, portland cement, 42.5MPa;shaft kiln
Use advice for data set When utilizing this data set, LCA practitioners should base their analysis on the functional unit of 1kg of cement with a 28-day compressive strength of 42.5MPa. Users should include emissions such as nitrogen oxides, sulfur dioxide, carbon dioxide, and dust in their impact assessment. The environmental impact of clay resource consumption and iron powder used as a corrective material should be omitted from the analysis at this stage. The methodological boundary includes raw meal preparation, clinker calcination, and cement production, and users should carefully consider the technological applicability of the shaft kiln which is specific to this regional industry.
Technical purpose of product or process This specific portland cement, characterized by a 28-day compressive strength of 42.5MPa, is suited for general construction purposes including infrastructure, buildings, and civil engineering projects that require a high grade of structural integrity. Its production process using a shaft kiln is particularly relevant to the region of Heilongjiang Province in the context of the current technological capabilities of the cement industry.
Classification
Class name : Hierarchy level
  • ILCD: Unit processes / Materials production / Other mineralic materials
General comment on data set Shaft kiln is used for the production of portland cement. A study was conducted on the process flow and operating parameters of the rotary kiln technology currently available in the cement industry in Heilongjiang Province, and input and output data of the established product system were collected and calculated and quantified.
Copyright No
Owner of data set
Quantitative reference
Reference flow(s)
Technological representativeness
Flow diagram(s) or picture(s)
  • NK0Hb2UOgows9vxHdZic8RrUn8d.png Image
Mathematical model
Model description The functional unit is the performance of 1kg cement with a 28-day compressive strength of 42.5MPa, that is, 1Fu=42.5kgMPa. The scope of evaluation is raw meal preparation, clinker calcination and cement preparation. The environmental load caused by the consumption of clay resources is not considered for the time being. Iron powder is an iron correction material, and its environmental impact will not be considered. The wastes considered to be emitted at the output end of the product system mainly include nitrogen oxides, sulfur dioxide, carbon dioxide and dust.
LCI method and allocation
Type of data set Unit process, black box
Deviation from LCI method principle / explanations None
Deviation from modelling constants / explanations None
Data sources, treatment and representativeness
Deviation from data cut-off and completeness principles / explanations None
Deviation from data selection and combination principles / explanations None
Deviation from data treatment and extrapolations principles / explanations None
Data source(s) used for this data set
Completeness
Completeness of product model No statement
Validation
Type of review
Dependent internal review
Reviewer name and institution
Data generator
Data set generator / modeller
Data entry by
Time stamp (last saved) 2024-03-19T21:18:09+08:00
Publication and ownership
UUID dcffcc2b-d964-46d2-94ed-0c7b3c5b0c75
Date of last revision 2024-04-20T14:40:39.845003+08:00
Data set version 00.01.005
Permanent data set URI https://lcadata.tiangong.world/showProcess.xhtml?uuid=dcffcc2b-d964-46d2-94ed-0c7b3c5b0c75&version=01.00.000&stock=TianGong
Owner of data set
Copyright No
License type Free of charge for all users and uses

Inputs

Type of flow Classification Flow Location Mean amount Resulting amount Minimum amount Maximum amount
Product flow
Materials production / Other mineralic materials 1137.5 kg1137.5 kg
General comment Limestone
Product flow
Materials production / Other mineralic materials 59.3 kg59.3 kg
General comment Gypsum
Product flow
Energy carriers and technologies / Hard coal based fuels 204.82 kg204.82 kg
General comment Standard coal. The original data is 0.1903kg standard coal, here converted to hard coal, the conversion formula is 1kg hard coal = 0.929kg standard coal.
Product flow
Energy carriers and technologies / Electricity 357.48 MJ357.48 MJ
General comment Electricity

Outputs

Type of flow Classification Flow Location Mean amount Resulting amount Minimum amount Maximum amount
Elementary flow
Emissions / Emissions to air / Emissions to air, unspecified 0.64 kg0.64 kg
General comment Dust, with an unspecified particle size, is treated as PM > 10 micrometers in diameter.
Elementary flow
Emissions / Emissions to air / Emissions to air, unspecified 0.4662 kg0.4662 kg
General comment Sulfur dioxide.
Elementary flow
Emissions / Emissions to air / Emissions to air, unspecified 1.602 kg1.602 kg
General comment Nitrogen oxides
Elementary flow
Emissions / Emissions to air / Emissions to air, unspecified 1092.8 kg1092.8 kg
General comment Carbon dioxide
Product flow
Materials production / Other mineralic materials 1000.0 kg1000.0 kg
General comment 1kg of Portland cement with a strength grade of 42.5.