Use advice for data set When utilizing this LCA data for the cement production process, ensure that the data corresponds accurately to the new dry process kiln technology. In modeling the cement production lifecycle, exclude the environmental load caused by the consumption of clay resources and the environmental impact due to the use of iron powder as a correction material. Consider the emissions of nitrogen oxides, sulfur dioxide, carbon dioxide, and dust in the impact assessment, as these are significant pollutants emitted from the cement production. The functional unit of the dataset is based on 1kg of cement with a 28-day compressive strength of 42.5MPa.
Technical purpose of product or process The portland cement produced using the new dry process kiln technology is utilized mainly in the construction industry. It is suitable for constructing infrastructures such as buildings, highways, and bridges where a high level of durability and strength is required. The cement, with a specified 28-day compressive strength of 42.5MPa, is appropriate for structural concrete and other applications where 42.5MPa of strength is necessary.
Classification
Class name : Hierarchy level
  • ILCD: Unit processes / Materials production / Other mineralic materials
General comment on data set New dry process kiln is used for the production of portland cement. A study was conducted on the process flow and operating parameters of the new dry-process technology currently available in the cement industry in Heilongjiang Province, and input and output data of the established product system were collected and calculated and quantified.
Copyright No
Owner of data set
Quantitative reference
Reference flow(s)
Technological representativeness
Flow diagram(s) or picture(s)
  • MSPWbT0ytoX9vbx6j29cuUHonYc.png Image
Mathematical model
Model description The functional unit is the performance of 1kg cement with a 28-day compressive strength of 42.5MPa, that is, 1Fu=42.5kgMPa. The scope of evaluation is raw meal preparation, clinker calcination and cement preparation. The environmental load caused by the consumption of clay resources is not considered for the time being. Iron powder is an iron correction material, and its environmental impact will not be considered. The wastes considered to be emitted at the output end of the product system mainly include nitrogen oxides, sulfur dioxide, carbon dioxide and dust.
LCI method and allocation
Type of data set Unit process, black box
Deviation from LCI method principle / explanations None
Deviation from modelling constants / explanations None
Data sources, treatment and representativeness
Deviation from data cut-off and completeness principles / explanations None
Deviation from data selection and combination principles / explanations None
Deviation from data treatment and extrapolations principles / explanations None
Data source(s) used for this data set
Completeness
Completeness of product model No statement
Validation
Type of review
Dependent internal review
Reviewer name and institution
Data generator
Data set generator / modeller
Data entry by
Time stamp (last saved) 2024-03-19T21:18:09+08:00
Publication and ownership
UUID 47999da2-6d54-4af2-a11d-47ca84c3da76
Date of last revision 2024-04-20T14:40:42.232438+08:00
Data set version 00.01.005
Permanent data set URI https://lcadata.tiangong.world/showProcess.xhtml?uuid=47999da2-6d54-4af2-a11d-47ca84c3da76&version=01.00.000&stock=TianGong
Owner of data set
Copyright No
License type Free of charge for all users and uses

Inputs

Type of flow Classification Flow Location Mean amount Resulting amount Minimum amount Maximum amount
Product flow
Materials production / Other mineralic materials 1104.4 kg1104.4 kg
General comment Limestone
Product flow
Materials production / Other mineralic materials 58.7 kg58.7 kg
General comment Gypsum
Waste flow
Wastes 319.4 kg319.4 kg
General comment Fly ash
Product flow
Energy carriers and technologies / Hard coal based fuels 100.526 kg100.526 kg
General comment Standard coal. The original data is 0.0934kg standard coal, here converted to hard coal, the conversion formula is 1kg hard coal = 0.929kg standard coal.
Product flow
Energy carriers and technologies / Electricity 343.8 MJ343.8 MJ
General comment Electricity

Outputs

Type of flow Classification Flow Location Mean amount Resulting amount Minimum amount Maximum amount
Elementary flow
Emissions / Emissions to air / Emissions to air, unspecified 0.324 kg0.324 kg
General comment Dust, with an unspecified particle size, is treated as PM > 10 micrometers in diameter.
Elementary flow
Emissions / Emissions to air / Emissions to air, unspecified 0.3893 kg0.3893 kg
General comment Sulfur dioxide
Elementary flow
Emissions / Emissions to air / Emissions to air, unspecified 1.557 kg1.557 kg
General comment Nitrogen oxides
Elementary flow
Emissions / Emissions to air / Emissions to air, unspecified 813.1 kg813.1 kg
General comment Carbon dioxide
Product flow
Materials production / Other mineralic materials 1000.0 kg1000.0 kg
General comment Portland cement with a strength grade of 42.5.